Mixes for BF runners

Ramming and castable runner mixes
Product Ferrorun ramming mix Ferrocast BF Ferrorun SX
Application Ramming mix for runner Castable runner mix Ramming mix for slag runner
Chemical Analysis, % SiO2 8-10% 8-10% 35-40%
Al2O3 55%, min 60%, min 0.5%, max
SiC 20%, min 20%, min
Fe2O3 1.5%, max 1.5%, max 1.5%, max
C 5%, min 5%, min 5%, min
CaO 2.5%, max
Grain size, mm 0-7 0-7 0-6
Density, kg/lt
Cold crushing strength kg/cm2 at 110°C 80 200 70